Phone : +0086-0411-88708355
Products   >   Boron nitride compound ceramic
Coating Crucibles

Independently developed, our new formula products address challenges such as sputtering pot issues and corrosion of nickel and copper. Through advanced formulation technology, components are optimized to ensure excellent chemical stability and stable resistivity. These products also offer exceptional oxidation resistance, effectively combating corrosion from aluminum, nickel, copper, and gold. With a maximum operating temperature of 1800°C, they are well-suited for demanding applications.

tem Number: BN-B/ BN-C/ BN-D/ BN-E
Purity (%)
BN+Zr+Al/ BN+SiC/ BN+Zr/ BN+AlN
Temperature
(Inert) 1800 °C max. under a protective gas environment
(vacuum) 1800°C max. under vacuum
(Air)1000°C max in the air

As boron nitride is a machinable ceramic material, we can craft it to your specifications within approximately 2 weeks based on the provided drawings. Please click ‘inquiry’ to send us a message and, if needed, email a drawing.

 

 

 

PRODUCT DESCRIPTION

Technical Properties

           Grade
Typical Value 

BN-B

BN-C

BN-D

BN-E

Purity (%)

BN+Zr+Al

BN+SiC

BN+Zr

BN+AlN

Color

Gray white

Gray green

Gray white

Gray green

Density (g/cm3)

2.25-2.35

2.40-2.50

2.80-2.90

2.80-2.95

Oxygen content (%)

Volume resistivity (Ω・cm

>1013

>1012

>1012

>1013

Operating temp
(℃)

  Air

≦1000

≦1000

≦1000

≦1000

 Inert gas

≦1750

≦1750

≦1800

≦1800

 Vacuum

≦1750

≦1750

≦1800

≦1800

Bending strength (MPa)

65

80

90

90

Coefficient of thermal expansion (10-6/℃)

2.0

2.8

3.0

2.8

Thermal conductivity (W/m・K)

30

40

30

85

● The data listed on this sheet are representative values and not guaranteed values.
● Please confirm the safety of use at your own responsibility.
● Dispose of the product in accordance with the law.
● The contents of this sheet may be updated without prior notice due to new information.

The important properties

1. Independently developed new formula products to solve the problems of sputtering pot and nickel and copper corrosion.

2. Adopt advanced formulation technology, optimize components, have good chemical stability and stable resistivity.

3. Good oxidation resistance, resistant to aluminum, nickel, copper, and gold corrosion.

4. The maximum using temperature is 1800 ℃.

MESSAGE